EVACOAT WASH PRIMER KS M 6030 Class 4 wash primer(2K)

usage
Pretreatment primer for industrial steel and non-ferrous metals (galvanizing, aluminum, etc.)

This paint is a two-component wash primer manufactured using excellent rust-preventive pigments that do not contain epoxy resins and harmful heavy metals.
It has excellent temporary rust prevention and substrate adhesion, and has good adhesion with the subsequent coating and top coating, so it is a paint suitable for KS M 6030 4 types as a pretreatment primer for general industrial and industrial facilities.

specification

Paint type
Epoxy polyamide / KS M 6030 Class 4 wash primer(Two-Component)
Drying time
Drying time
Category 5℃ 20℃ 30℃
Set-to-touch 40 minutes 30 minutes 20 minutes
Dry-hard 1 hour 40 minutes 30 minutes
Over-coat (Min.) 4 hours 2 hours 1 hour
Over-coat (Max.) 30 days 15 days 7 days
Pot life 16 hours 12 hours 8 hours
Thinner
General coating : DR-100
Dilution ratio
▷Brush, roller, spray coating: less than 5%
Specific gravity
Approx. 1.3(Based on gray color)
Theoretical Coverage
25㎡/ℓ (1time - 15㎛)
Solid volume ratio
Approx. 38±1%
Color
Gray, redbrown, ordered colors
Thickness of dried film
10~20㎛
Mixing ratio
Base(A)/Hardener(B)=3/1 (Volume ratio)
Flash point
At least 7℃
Gloss
Matte
Shelf life
12 months (Dry, cool, and dark place with good ventilation)

how to use

Surface treatment
1. Completely remove oil, moisture, sand, dust, and other foreign matter from the surface to be coated.
2. Paint the steel immediately after processing.
3. High gloss and smooth galvanized steel sheets (such as deck plates) require a test coat. To increase adhesion, surface treatment with sandpapering is recommended if necessary.
Coating method
1. Coating can be done by either brush, air or airless spray coating.
2. Airless spray coating:
- Tip diameter : 0.013"~0.017"
- Injection pressure : 1500~2000 PS.I(105~140㎏/㎠)
- Store the coating equipment after cleaning with an exclusive thinner immediately after use.
Preceding and follow-up coating
1. Follow-up coating : Epoxy resin, urethane resin, alkyd resin, fluororesin top coat
Remarks
1. Sufficient performance after last coating is achieved after drying for 7 days at 20℃.
2. For coating areas exposed to the outside, yellowing and chalking may occur in a short period of time due to the effect of sunlight. Upon coating for areas exposed to the outside, be sure to apply top coating.
3. Apply the dry film with the recommended thickness of dried film.